特性:玻璃15%强化,一般用途。性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | 基本性能 | 吸水率 | 23℃,24小时 | ASTM D-570 | | % | 物理性能 | 泰伯磨耗量 | (1000g,CS-17)23℃ | ASTM D-1044 | | mg/1000次 | 比重 | | ASTM D-792 | | | 机械性能 | 抗剪强度 | 80℃ | ASTM D-732 | | Kg/cm2 | IZOD冲击强度 | V-缺口1/2,23℃ | ASTM D-256 | | kg·cm/cm2 | 抗拉屈服强度 | 23℃ | ASTM D-638 | | Kg/cm2 | 抗剪强度 | 23℃ | ASTM D-732 | | Kg/cm2 | 断裂伸长率 | 23℃ | ASTM D-638 | | % | 挠曲模量 | -40℃ | ASTM D-790 | | Kg/cm2 | 洛氏硬度 | 23℃ | ASTM D-785 | | M-标度 | 洛氏硬度 | 23℃ | ASTM D-785 | | R-标度 | 抗拉断裂强度 | 23℃ | ASTM D-638 | | Kg/cm2 | 断裂伸长率 | -40℃ | ASTM D-638 | | % | 断裂伸长率 | 80℃ | ASTM D-638 | | % | 挠曲强度 | 80℃ | ASTM D-790 | | Kg/cm2 | 挠曲强度 | 23℃ | ASTM D-790 | | Kg/cm2 | 挠曲强度 | -40℃ | ASTM D-790 | | Kg/cm2 | 抗拉屈服强度 | -40℃ | ASTM D-638 | | Kg/cm2 | 抗拉屈服强度 | 80℃ | ASTM D-638 | | Kg/cm2 | 挠曲模量 | 23℃ | ASTM D-790 | | Kg/cm2 | 挠曲模量 | 80℃ | ASTM D-790 | | Kg/cm2 | 电气性能 | 介电强度 | 1/8" | ASTM D-149 | | KV/mm | 体积电阻率 | | ASTM D-257 | | Ω.cm | 热性能 | 热挠曲温度 | 18.6kg/cm2 | ASTM D-648 | | ℃ | 比热 | | | | Cal/g·℃ | 线性热膨胀系数 | | ASTM D-696 | | ×10-5cm/cm/℃ | 热挠曲温度 | 4.6kg/cm2 | ASTM D-648 | | ℃ | 熔点 | | 差示扫描测热计DSC | | ℃ | 其它性能 | 强化含量 | | | | WT% |
|